MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Quantum PEI - Ultem®
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes:

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.27 g/ccASTM D792
Water Absorption 0.25 %ASTM D570
Water Absorption at Saturation 1.25 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 109ASTM D785
Hardness, Rockwell R 123ASTM D785
Hardness, Shore D 93ASTM 2240
Tensile Strength 15200 psiASTM D638
Elongation at Break 60 %ASTM D638
Tensile Modulus 430000 psiASTM D638
Flexural Strength 22000 psiASTM D790
Flexural Modulus 480000 psiASTM D790
Compressive Strength 22000 psiASTM D695
Compressive Modulus 480000 psiASTM D695
Shear Strength 15000 psiASTM D732
Izod Impact, Notched 1.00 ft-lb/inASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+17 ohm-cmASTM D257
Dielectric Constant 3.15
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 830 V/milASTM D149
Dissipation Factor 0.0010
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 31.0 µin/in-°FASTM D696
Thermal Conductivity 1.00 BTU-in/hr-ft²-°FASTM C177
Melting Point 460 °FASTM D3417
Maximum Service Temperature, Air 340 °F
Deflection Temperature at 0.46 MPa (66 psi) 410 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 392 °FASTM D648
Flammability, UL94 V-0
 
Compliance PropertiesOriginal ValueComments
FDA Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Quantum PEI - Ultem® 30% Glass Fiber Filled
Ensinger TECAPEI® made from Ultem® 1000 PEI
Overview of materials for Polyetheretherketone, Unreinforced
Proto3000 ULTEM* 9085 Fused Deposition Modeling Polymer
3D Systems Fused Deposition Modeling Material ULTEM

PQUANTU013 / 160437

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.