MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Innospec FLEXAREN® 07000 EVA-Copolymer
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Film Grade

Material Notes: CAS Number: 24937-78-8

FLEXAREN® 07000 is a high quality ethylene vinyl acetate copolymer with 7 % content of vinyl acetate. The product is manufactured by high pressure tubular process. FLEXAREN® 07000 is more elastic than LDPE and compatible with a wide range of polymers. It can be processed with the same equipment.

Application:

  • Stretch films
  • Flexible hoses
Properties:
  • Flexibility – especially at low temperatures
  • Good mechanical properties

Information provided by Innospec Inc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.925 g/ccDIN EN ISO 1183-1
Vinyl Acetate Content 7.0 %FTIR
Melt Flow 0.40 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 95ISO 868
Hardness, Shore D 42ISO 868
Tensile Strength at Break 19.0 MPaISO 527 (PK 1 BA)
Elongation at Break >= 700 %ISO 527 (PK 1 BA)
50% Modulus 0.00650 GPa
@Strain 50 %
ISO 527 (PK 1 BA)
Film Tensile Strength at Break, MD 27.0 MPaISO 527
Film Tensile Strength at Break, TD 24.0 MPaISO 527
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 75.0 °CISO 306 Method A
 
Processing PropertiesOriginal ValueComments
Processing Temperature 120 - 160 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Innospec FLEXAREN® 14003 EVA-Copolymer
Innospec FLEXAREN® 07002 EVA-Copolymer
Honeywell A-C® 400A EVA copolymer
LG Chemical SEETEC EF221 Ethylene Vinyl Acetate
Versalis Greenflex® FD 50 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion

PINOS001 / 183444

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.