MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Arkema KYNAR FLEX® 3120-50 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF); Polyvinylidinefluoride (PVDF), Molded/Extruded

Material Notes: Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, 150°C temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistance; high purity

Applications:

  • Chemical processing – production, storage and transfer of corrosive fluids
  • Electronics – protective sheathing, plenum and wiring insulation
  • Semi-conductor industry
  • Food stuff and Healthcare industries
  • Transportation – fuel line and pipe, thermoformed body components

Information provided by Arkema Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.75 - 1.77 g/ccASTM D792
Density 1.78 g/ccISO 1183
Water Absorption 0.030 %Dry; Sim. to ISO 62
 0.030 - 0.050 %ASTM D570
Viscosity 2.00e+6 - 2.60e+6 cP
@Shear Rate 100 1/s,
Temperature 230 °C
Melt; ASTM D3835
Melt Flow 0.50 g/10 min
@Load 12.5 kg,
Temperature 230 °C
cm³/10 min Volumetric Rate; ISO 1133
 2.5 - 7.5 g/10 min
@Load 12.5 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65 - 70ASTM D2240
Tensile Strength at Break 34.5 - 48.3 MPaASTM D638
Tensile Strength, Yield 27.0 MPaDry; ISO 527-1/-2
 24.1 - 34.5 MPaASTM D638
Elongation at Break >= 50 %Dry; ISO 527-1/-2
 300 - 500 %ASTM D638
Elongation at Yield 10 - 20 %ASTM D638
 15 %Dry; ISO 527-1/-2
Tensile Modulus 700 MPaDry; ISO 527-1/-2
 689 - 1170 MPaASTM D638
Flexural Strength 20.7 - 34.5 MPa
@Strain 5.0 %
ASTM D790
Flexural Modulus 621 - 827 MPaASTM D790
Compressive Strength 31.0 - 41.4 MPaASTM D695
Izod Impact, Notched NBASTM D256
Izod Impact, Unnotched NBASTM D256
Charpy Impact, Notched NB
@Temperature 23.0 °C
Dry; ISO 179/1eA
Coefficient of Friction, Dynamic 0.30vs. steel; ASTM D1894
Coefficient of Friction, Static 0.31vs. steel; ASTM D1894
Taber Abrasion, mg/1000 Cycles 16 - 19CS 17 1000g:pad; ASTM-G195-13A
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 5.30e+11 - 5.50e+11 ohmASTM D257
Dielectric Constant 3.2 - 10.2
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 1.30 - 1.50 kV/mmASTM D149
Dissipation Factor 0.020 - 0.19
@Frequency 100000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 126 - 185 µm/m-°CASTM D696
Specific Heat Capacity 0.745 - 0.958 J/g-°CDSC
Thermal Conductivity 0.144 - 0.180 W/m-KASTM D433
Melting Point 161 - 168 °CASTM D3418
 165 °C10°C/min; Dry; ISO 11357-1/-3
Maximum Service Temperature, Air 150 °CUL RTI
Deflection Temperature at 0.46 MPa (66 psi) 54.4 - 76.7 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 43.3 - 54.4 °CASTM D648
 50.0 °CDry; ISO 75-1/-2
Glass Transition Temp, Tg -41.1 - -39.4 °CASTM D7028
 -40.0 °C10°C/min; Dry; ISO 11357-1/-2
Decomposition Temperature 375 °C1% wt. loss, TGA, in air
 410 °C1% wt. loss, TGA, in nitrogen
UL RTI, Electrical 150 °CUL 746B
UL RTI, Mechanical without Impact 150 °CUL 746B
Flammability, UL94 V-0
@Thickness 1.00 mm
Yellow Card Available; Dry; IEC 60695-11-10
 V-0
@Thickness 1.50 mm
Yellow Card Available; Dry; IEC 60695-11-10
 5VA
@Thickness 1.00 mm
IEC 60695-11-20
Oxygen Index 42 %ASTM D2863
 43 %Dry; ISO 4589-1/-2
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.41sodium D line; ASTM D542
 
Processing PropertiesOriginal ValueComments
Processing Temperature 225 °CCompression Molding; Molding Temperature; ISO 293
 
Descriptive Properties
Compression Molding Demolding Temperature (°C)120ISO 293
Compression Molding Time3 min.ISO 293
Form as DeliveredPellets
Heat StabilizedYes
Light StabilizedYes
Moisture SensitiveNo
Processing MethodsOther Extrusion
 Profile Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema Kynar Flex® PPA 2200 PVDF
Arkema KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Arkema KYNAR FLEX® 2950-05 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Arkema KYNAR FLEX® 2850-07 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Arkema KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion

PARKG926 / 144551

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.