D4052-F is a fractional-melt low density formulation with low slip and low antiblock. It is suggested for film applications requiring impact strength, outstanding clarity, and good tear resistance. This product is suggested for packaging frozen foods and for similar applications requiring toughness and clarity. Information from manufacturer data sheet. Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line. |
Impact strength, outstanding clarity, and good tear resistance |