MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Toyobo Pibiflex® 3564T Thermoplastic Copolyester Elastomer
Categories: Polymer; Thermoplastic; Polyester, TP; Polyester Thermoplastic Elastomer

Material Notes: Product Description: Pibiflex 3564T is a nominal 38 Shore D thermoplastic polyester elastomer with medium modulus and improved flow for general use with improved heat resistance.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 g/cc0.0401 lb/in³ISO 1183
Water Absorption at Saturation 0.60 %0.60 %ISO 62
Maximum Moisture Content 0.0500.050
Melt Flow 25 g/10 min
@Load 2.16 kg,
Temperature 220 °C
25 g/10 min
@Load 4.76 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 35
@Time 15.0 sec
35
@Time 0.00417 hour
ISO 868
Tensile Strength at Break 18.0 MPa2610 psiISO 527-2/50
Elongation at Break >= 500 %>= 500 %ISO 527-2/50
Tensile Modulus 0.0500 GPa7.25 ksiISO 527-1
Flexural Modulus 0.0500 GPa7.25 ksiISO 178
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
 NB
@Temperature 22.8 °C
NB
@Temperature 73.0 °F
ISO 179/1eU
Charpy Impact, Notched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eA
 NB
@Temperature 22.8 °C
NB
@Temperature 73.0 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 195 °C383 °FISO 11357-3
 
Processing PropertiesMetricEnglishComments
Drying Temperature 100 - 110 °C212 - 230 °F
Dry Time 4.00 hour4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHCQ6295 / 310988

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.