MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Methode 9101 Conductive Inkjet Ink
Categories: Other Engineering Material; Ceramic/Metallic Coating

Material Notes: An aqueous silver nano particle ink designed for both thermal and piezo inkjet printing systems. The ink is water based and RoHS compliant. Good electrical resistance is achieved without the need for secondary curing or additional processing when printed on coated polymer films and papers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³
Filler Content 0.00 %0.00 %Silver (Ag)
Particle Size 0.10 µm0.10 µm
Viscosity 3.0 - 10 cP3.0 - 10 cP
Surface Tension 45 - 50 dynes/cm45 - 50 dynes/cm
 
Descriptive Properties
Adhesionpasses tape test
Conductive Filler TypeSilver (Ag)
Material TypeReady-To-Use Formulation
Recommended Substratesink receptive coated polyester, paper, polyethylene, etc.
Solvent SystemWater based

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFLEXCM33 / 179435

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.