Epoxy Phenol Novolac resin adduct with 1300X13 CTBN with 2.3 functionality. Increases toughness, impact resistance, and peel adhesion for medium-viscosity, higher Tg, epoxy phenol novolac systems.Information provided by Emerald Performance Materials. |