Celanex 2000-3FC is a general purpose, unreinforced PBT with a good balance of mechanical properties and processabillity for use in food contact applications.. Celanex 2000-3FC is a high flow material. Celanex 2000-3FC contains an internal lubricant for improved mold release.Information provided by Celanese |