MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Suzhou Hipro Polymers Hiprolon® 200 MC HLS G30 Nylon 1010, 30% glass fiber filled  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Hiprolon® 200 MC HLS G30 is a polyamide 10.10 compound reinforced with 30% chopped glass fiber for injection molding; features high dimension stability, chemical resistance, impact resistance, low friction, high flow ability; widely used for auto parts, thin wall housing, machinery & sports equipment et al;

Information provided by Suzhou Hipro Polymers Co. Ltd., subsequently acquired by Arkema S.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.27 g/ccISO 1183
Water Absorption 0.60 %ISO 62
Linear Mold Shrinkage 0.0015 cm/cmnormal; ISO 294-4,2577
Linear Mold Shrinkage, Flow 0.0065 cm/cmISO 294-4,2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 136 MPaISO527-2/1A
Elongation at Break 5.0 %ISO 527-2/1A
Tensile Modulus 7400 MPaISO 527-1/-2
Charpy Impact Unnotched 95.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
 95.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 11.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 19.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+17 ohm-cmISO 60695
Comparative Tracking Index >= 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 202 °CISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 195 °CISO 75-1/2
Deflection Temperature at 1.8 MPa (264 psi) 185 °CISO 75-1/2
Vicat Softening Point 190 °CISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
IEC60695
 HB
@Thickness 3.20 mm
IEC60695
 
Processing PropertiesOriginal ValueComments
Melt Temperature 240 - 290 °C
Mold Temperature 60.0 - 110 °C
Drying Temperature 80.0 - 90.0 °C
Dry Time 4 hour
Injection Pressure 70.0 - 130 MPa

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Suzhou Hipro Polymers Hiprolon® 70 MC HLS G30 Nylon 610, 30% glass fiber filled
RheTech Products GC15P200-01 15% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Arkema Rilsan® TMVO PA1010
Suzhou Hipro Polymers Hiprolon® 200 NN Nylon 1010, dry
3M FM1183 Indoor UL Recognized MC Polyester Label Products

PHIPRO15 / 106830

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.