MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
INEOS Styrolution Lustran® EHI-7 Acrylonitrile Butadiene Styrene (ABS)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Extruded; Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded

Material Notes: Terluran® EHI-7 is a medium flow, high impact extrusion grade with super high gloss and superior surface aesthetics. Styrolution’ s Terluran® EHI-7 is intended for mono or multilayer sheet making it a perfect fit as a substrate for our weatherable Luran® S ASA. Features: High Impact, High gloss, Outstanding deep draw ability for thermoforming applications, Excellent chemical resistance, Excellent colorability, Enhanced depth of image. Applications: Sheet extrusion, Thermoforming, Excellent chemical resistance, Coextrusion with Luran® S ASA

Information provided by Styrolution.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/ccASTM D 792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cmASTM D 955
Melt Flow 7.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 43.7 MPaASTM D 638
Elongation at Break 9.2 %ASTM D 638
Elongation at Yield 2.9 %ASTM D 638
Tensile Modulus 2170 MPaASTM D 882
Flexural Yield Strength 0.379 MPa
@Strain 5.0 %
ASTM D 790
Flexural Modulus 2040 MPaASTM D 790
Izod Impact, Notched 7.10 ft-lb/in
@Temperature 23.0 °C
ASTM 256
Falling Dart Impact 22.8 ft-lbInstrumented, Peak force; ASTM D 3763
 36.0 ft-lbInstrumented, total energy; ASTM D 3763
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 99.0 °Cunannealed; ASTM D 648
Vicat Softening Point 100 °C
@Load 1.02 kg
VST/A/50. 50C/h; ISO 306
 
Optical PropertiesOriginal ValueComments
Gloss 92 %at 60°, specular; ASTM D 523
 
Processing PropertiesOriginal ValueComments
Melt Temperature 218 - 260 °C
Mold Temperature 29.0 - 60.0 °C
Drying Temperature 79.0 °C
@Time 7200 - 14400 sec
 
Descriptive Properties
Suggested Max Regrind, %20

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSTYR9914 / 216138

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.