MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polykemi AB POLYfill PPH FR15030 XNH Polypropylene Homopolymer, Flame Retardant, Halogen Free
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Flame Retardant

Material Notes:

Information provided by Polykemi AB

Key Words: Polypropylene Homopolymer
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.90 g/cc0.0686 lb/in³ISO 1183
Melt Index of Compound 15 g/10 min
@Load 2.16 kg,
Temperature 230 °C
15 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 73
@Time 15.0 sec
73
@Time 0.00417 hour
Polykemi
Tensile Strength at Break <= 28.0 MPa<= 4060 psiISO/R527
Elongation at Yield 6.0 %6.0 %ISO/R527
Flexural Strength <= 55.0 MPa<= 7980 psiISO 178
Flexural Modulus 2.20 GPa
@Temperature 23.0 °C
319 ksi
@Temperature 73.4 °F
ISO 178
Charpy Impact, Notched  0.200 J/cm²
@Temperature -20.0 °C
0.952 ft-lb/in²
@Temperature -4.00 °F
ISO 179
 0.350 J/cm²
@Temperature 23.0 °C
1.67 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 97.0 °C207 °F120°C/h; ISO 75/1
Deflection Temperature at 1.8 MPa (264 psi) 66.0 °C151 °F120°C/h; ISO 75/1
Vicat Softening Point  96.0 °C
@Load 5.001 kg
205 °F
@Load 11.03 lb
50°C/h; ISO 306
 150 °C
@Load 1.00 kg
302 °F
@Load 2.21 lb
50°C/h; ISO 306
Flammability, UL94 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
Glow Wire Test 960 °C
@Thickness 1.60 mm
1760 °F
@Thickness 0.0630 in
IEC 695-2-1
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 220 °C356 - 428 °F
Mold Temperature 20.0 - 50.0 °C68.0 - 122 °F
Drying Temperature 70.0 - 80.0 °C158 - 176 °F
Dry Time 2 - 4 hour2 - 4 hourin circulation dryer
 2 - 4 hour2 - 4 hourin desiccant air dryer
Injection Pressure 40.0 - 110 MPa5800 - 16000 psi
Back Pressure 0.500 - 1.00 MPa72.5 - 145 psi
 
Descriptive Properties
Holding Pressure20-40% of injection pressure
Injection SpeedNormal

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plastcom SLOVALEN PH 78 FRT 5 Polypropylene Homopolymer, Halogen Free and Phosphor Free Flame Retardant
Plastcom SLOVALEN PH 76 FRD 3 PP, flame retardant
Multibase Multi-Flam™ 0302 PP NH Polypropylene
Multibase Multi-Flam™ 0220 PP Polypropylene
Multibase Multi-Flam™ 0206 PP Polypropylene

PPOLYK339 / 123064

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.