MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Geon® Performance Solutions 130 Series 137 Polyvinyl Chloride Copolymer (PVC Copolymer)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Geon® 137 is a carboxyl functional copolymer dispersion resin providing extra adhesion to synthetic fabrics, such as nylon, allowing the elimination of adhesion promoters. It provides the ability to crosslink with epoxies, providing a more solvent resistant coating. The polarity of Geon® 137 allows its use in hydrosols. Geon® 137 is recommended for applications where special characteristics are requires, such as nylon fabric coating, hydrosol inks and coatings, solvent resistant coatings, and automotive sealants.

Note: The value set forth represent typical values and PolyOne Corporation, therefore, makes no representation that the material in any particular shipment will conform to the listed properties. Packaging: This resin is shipped in multi-wall paper bags, net weight 50 lbs, 2500 lbs per pallet. Information shown on the package includes commercial identification number, lot and weight. Geon® ALTC and ASTM D638 (formulation): 100phr Geon® 137, 77phr DINP, 3phr ESO, and 2phr Therm-Chek SP 120 LOHF Geon® STP 390(formulation): 100phr Geon® 137, and 60phr DOP

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.40 g/cc1.40 g/cc
Bulk Density 0.400 g/cc0.0145 lb/in³
Fineness 3.03.0Hegman, North Fineness; Geon® 390
Relative Viscosity 2.55 cP2.55 cPCorrelation, Cyclohexanone 1%; Internal Method
Brookfield Viscosity 16.3 cP16.3 cPInitial Viscosity @ 2 rpm; Geon® ALTC 22 (with provided formulation); Internal Method
 17.9 cP17.9 cPOne Day Viscosity @ 2 rpm; Geon® ALTC 22 (with provided formulation); Internal Method
 27 cP27 cPInitial Viscosity @ 20 rpm; Geon® ALTC 22 (with provided formulation); Internal Method
 32.3 cP32.3 cPOne Day Viscosity @ 20 rpm; Geon® ALTC 22 (with provided formulation); Internal Method
Viscosity Measurement 1.11.1Inherent; ASTM D1243-60-A
Melt Flow 12 g/10 min
@Pressure 0.655 MPa
12 g/10 min
@Pressure 95.0 psi
Severs Efflux; Geon® ALTC 23 (with provided formulation); Internal Method
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 14.8 MPa2150 psiOptimum; With provided formulation; ASTM D638
 
Optical PropertiesMetricEnglishComments
Gloss 55 %55 %60 Degree Fused 5 mins @ 350 F Geon® ALTC 65 (with provided formulation); Internal Method
Transmission, Visible 78 %78 %Geon® ALTC 66 (with provided formulation); Internal Method
 
Processing PropertiesMetricEnglishComments
Moisture Content 0.12 %0.12 %Karl FisherGeon® STP 683; Internal Method
 
Descriptive Properties
FeaturesGood Adhesion
 Solvent Resistant
Fixed Acid2.4%Internal Method; Geon® STP 1315
FormsPowderFine, White Powder
Free Acid0.4%Internal Method; Geon® STP 1315
Gel Temperature67 °CInternal Method; Geon® ALTC 29 (with provided formulation)
Generic MaterialPVC Copolymer
Generic NamePolyvinyl Chloride Copolymer (PVC Copolymer)
K-Value73Internal Method; Correlation, 0.5gm/100ml
Methanol Extractables3.1%Internal Method; Geon® STP 894
Polymerization ProcessMicrosuspension
Processing MethodCoating
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
Residual Vinyl Chloride Monomer< 9 ppmInternal Method; Geon® STP 1005
UsesAutomotive Applications
 Coating Applications
 Fabric Coatings
 Sealants

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Geon® Performance Solutions 130 Series 136 Polyvinyl Chloride Copolymer (PVC Copolymer)
Formosa Plastics Formolon® 113 PVC
Geon® Performance Solutions 130 Series 138 Polyvinyl Chloride Copolymer (PVC Copolymer)
Inovyn 460SL Polyvinyl Chloride grafted copolymer
Inovyn Vinidur® 464SZ Polyvinyl Chloride grafted copolymer

PH0POL0789 / 145358

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.