MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Min-K® 1302 Thermal Ceramic
Categories: Ceramic

Material Notes: Molded Min-K boards and shapes offer the thermophysical properties of Min-K insulation in easily handled boards and shapes. Molded Min-K insulation is made in two standard types: 1302 and the High Purity TE series. These materials can also be in specified shapes, molded to close dimensional tolerances in sizes and thicknesses consistent with pressure and heat-molding techniques. Molded Min-K insulation has been used successfully in manned spacecraft, aircraft, and other high-temperature applications where low thermal conductivity plus space and weight savings are a critical consideration. This includes steady-state and transient applications. Min-K 1302 is a microporous material specifically designed to be molded into block and machined to specific customer designs.

Applications: Aerospace, High temperature, Instrumentation and analytical equipment

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 55.0 psi
 110 psi5% compression
 190 psi8% compression
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0300 W/m-K
@Temperature 149 °C
between hot surface and cold surface; ASTM C-518
 0.0320 W/m-K
@Temperature 204 °C
between hot surface and cold surface; ASTM C-518
 0.0330 W/m-K
@Temperature 316 °C
between hot surface and cold surface; ASTM C-518
 0.0360 W/m-K
@Temperature 427 °C
between hot surface and cold surface; ASTM C-518
 0.0390 W/m-K
@Temperature 538 °C
between hot surface and cold surface; ASTM C-518
 0.0530 W/m-K
@Temperature 649 °C
between hot surface and cold surface; ASTM C-518
Maximum Service Temperature, Air <= 982 °C
Shrinkage 0.50 %
@Treatment Temp. 982 °C,
Time 14400 sec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Min-K® K-Shield™ Felt AG Composite Thermal Ceramic
Morgan Advanced Ceramics Min-K® TE 1400 Thermal Ceramic
Morgan Advanced Ceramics Min-K® TE 1800 Thermal Ceramic
Morgan Advanced Ceramics AL 1009™ Mac-A100W-Porous Aluminum Oxide Ceramic
Morgan Advanced Ceramics Cerox® 730 Thermal Ceramic

CMORF6126 / 202910

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.