MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Synthos ACM2228S Acrylic Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Acrylic Rubber has excellent aging resistance, oil resistance, high temperature resistance and ozone resistance. Widely used in fields such as automobiles and motorcycles.

Introduction: “SUNACR” is the registered trade-name of Acrylic rubber (ACM) produced by Sundow Polymers Co., Ltd. SUNACRACM rubber is a high-performance rubber prepared by lotion polymerization. It has excellent aging resistance, oil resistance, high temperature resistance and ozone resistance is suitable for making rubber hoses, oil seals, rubber gasket ,etc. Which is widely used in automobiles, motorcycles, ships, electric power and other fields. SUNACRACM rubber can be used to replace AEM rubber.

Application: ACM Rubber is widely used in various high temperature and oil resistant environments and has become a sealing material developed and promoted in the automotive industry in recent years.

  • high temperature oil seals
  • gaskets
  • hoses
  • hydraulic oil hoses
  • transmission seal
  • corrugated pipe

Information provided by Sundow Polymers Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Mooney Viscosity 39 - 49
@Temperature 100 °C
ML(1+4)
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg -28.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSUNDOW009 / 320040

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.