Superwool ® HT LB™ VF is a tailored product, flexible, offers a good resistance and facilitates installation in which, rigid products are not suitable. Typical applications: - Riser sleeves and crucibles for ferrous and non ferrous molten metals
- Stopper nut insulation
- Ladle shroud gasket
- Nozzle insulation in continuous casting
- Roller inserts in roller hearth furnace
- Glass casting mould
- Tube insulation end in tube fumes boiler
- Insulation for domestic appliance
- Furnace insulation