MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ArcelorMittal IF 180 High strength IF steel, Cold rolled
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Available in the following: uncoated (HC180Y), electroglavanized (HC180Y+ZE) and Extragal®/Galvannealed (HX180YD+Z/+ZF)

Description: These steels were designed to provide an excellent combination of drawability and mechanical strength based on their specific interstitial free (IF) metallurgy. IF180 offers drawability similar to that of ArcelorMittal 04 combined with tensile strength comparable to that of H220, for example. These steels are hardened by adding manganese, silicon and phosphorous in solid solution to the ferrite. The metallurgy of IF steels optimizes their drawability.

  • Their low YS/UTS ratio and high strain hardening coefficient n ensure excellent deep-drawability and good strain redistribution.
  • Their high strain ratio r ensures good deformation behavior, making them suitable for deep-drawing.
These steels are particularly suitable for complex parts requiring high mechanical strength, such as wheel arches, toe-boards, reinforcements, etc. These steels have high strain hardening potential during forming, lending deep-drawn parts (trunks, tailgates, doors, linings, wheel arches, etc.) good dent resistance. The IF180 to IF 260 grades can be used, with certain coatings, to manufacture visible parts such as door panels. The IF 300 grade is designed for more complex structural parts (longitudinal beams, cross members, suspension and chassis components, etc.).

Application: With their high mechanical strength guaranteeing good fatigue and impact resistance, these steels are intended for structural parts (longitudinal beams, cross members, B-pillars, etc.) as well as for skin parts, in which they provide good indentation resistance. In contrast to that of conventional drawing qualities, the weight reduction potential of these products increases with drawing depth.

Information provided by ArcelorMittal

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 340 - 400 MPa
Tensile Strength, Yield 180 - 230 MPa
Elongation at Break >= 35 %L0=80 mm, th<3 mm
Fatigue Strength <= 255 MPa
@# of Cycles 2.00e+6
 <= 255 MPa
@# of Cycles 1.00e+7
 <= 275 MPa
@# of Cycles 100000
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.010 %
Iron, Fe >= 98.74 %as balance
Manganese, Mn <= 1.0 %
Silicon, Si <= 0.25 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ArcelorMittal IF 300 High strength IF steel, Cold rolled
ArcelorMittal 180 BH Bake hardening steel, Cold rolled
ArcelorMittal 56 High formability steel for drawing, Cold rolled
ArcelorMittal 57 High formability steel for drawing, Cold rolled
Cadi MOLD-MORâ„¢ 1

NARCE054 / 159962

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.