MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Resin Technology Group TIGA 108 Room Temperature Curing Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: 1 to1 mix ratio by volume.

TIGA 108 is an epoxy adhesive system that provides excellent bond strength to most substrates. Recommended for production bonding applications, this low viscosity formulation can be easily dispensed and mixed in convenient one to one mix ratios. TIGA 108 is a gap fill adhesive which forms water resistant bonds, therefore is ideal for bonding applications where substrates will be subjected to water or high humidity environments for long periods of time.

Applications:

This product bonds well to iron, aluminum, bronze, brass, wood concrete, ceramic materials and glass. It maintains a resistance not only to water, but oil and gasoline as well. Cures to smooth glass like finish.

Information provided by Resin Technology Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/cc
Viscosity 19000 cP
@Temperature 25.0 °C
Mixed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 75
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 10 ohm-cm
Dielectric Constant 3.0
@Frequency 1e+6 Hz
Dielectric Strength >= 420 V/mil
Dissipation Factor 0.020
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 50.0 µm/m-°C
@Temperature 20.0 °C
Maximum Service Temperature, Air 135 °C
Minimum Service Temperature, Air -60.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 65.0 °C
 24.0 hour
@Temperature 25.0 °C
Pot Life 8.00 - 12.0 min
@Temperature 25.0 °C
 
Descriptive Properties
ColorClear, black, or white

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Resin Technology Group KONA 877 Low Viscosity, Low Shrinkage, Vacuum Grade Casting Resin
Resin Technology Group TIGA HTR-815 High Temperature Resistant, Rigid Thermally Conductive Epoxy
Resin Technology Group TIGA F-715 Rome Temperature Curing, Rigid Thermally Conductive Epoxy
Resin Technology Group TIGA 202-EX High Performance, Fast Cure Adhesive
Resin Technology Group KONA 871 Low Cost Epoxy Resin

PRESINT628 / 65512

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.