MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Shandong Dawn Dawnprene 20-45D TPV (EPDM/PP)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Uses: Automotive - Interior Parts: airbag frame

Information provided by Shandong Dawn Polymer Material Co.,Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.890 g/cc0.0322 lb/in³ISO 1183
Melt Flow 4.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
4.5 g/10 min
@Load 4.76 lb,
Temperature 446 °F
GB/T3682
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4444ISO 7619
Tensile Strength 13.0 MPa1890 psiISO 37
Elongation at Break 580 %580 %ISO 37
Flexural Strength 31.0 MPa4500 psiISO 178
Izod Impact, Notched (ISO) NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 180
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 51.0 °C124 °FISO 75
 
Descriptive Properties
Accelerated Weathering SAE J25271.6Delta E, 5 period
 3Ordo, 80°C 2hr
Elongation Change (%) ISO 188-18.8change @ heat aging 100°C, 1000hr
Fire Resistance (mm/min)20GB 8410
Fogging (mg)1.08DIN 75201
Tensile Change (%) ISO 188-15.6change @ heat aging 100°C, 1000hr
Volatile Organic CompoundsPassVDA278

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Shandong Dawn Dawnprene 20-55A TPV (EPDM/PP)
Celanese Celstran® PP-GF40-20 AD 3004 Black PP, 40% Glass Reinforced
ExxonMobil Santoprene® 101-87 Thermoplastic Elastomer
Polykemi AB POLYelast TPE EC90 D50 P05B Thermoplastic Elastomer, PP/EPDM
Shandong Dawn Dawnprene 11-40D TPV (EPDM/PP)

PSHAND943 / 192582

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.