MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Arkema Rilsan® Fine Powders 6189 YELLOW RDP 21 FB PA11
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 11 (PA11); Nylon 11, Powder

Material Notes:

Information provided by Arkema Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.18 - 1.23 g/cc1.18 - 1.23 g/ccCoating; ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Impact Test 160 J118 ft-lbImpact Resistance; ASTM D2794
Taber Abrasion, mg/1000 Cycles <= 25<= 25Wheel CS 17, load 1 kg; ASTM D1044
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 15.7 - 41.3 kV/mm
@Thickness 0.350 - 0.450 mm
399 - 1050 kV/in
@Thickness 0.0138 - 0.0177 in
ASTM D149
 
Thermal PropertiesMetricEnglishComments
Melting Point 183 - 193 °C361 - 379 °FISO 1218
 
Descriptive Properties
Approximate RAL number1021
ColorYellow
Covering Efficiency (kg/m²)0.35
Covering Efficiency, Thickness (µm)300
Grade Package Weight - Drums (lb/drum)100
Moisture SensitiveNo

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PARKF563 / 291241

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.