MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics Firecrete 97 Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Tabular Alumina. Bond type: Hydraulic.

Description: A high purity tabular alumina-based casting concrete with very low iron and silica content for service above 1800°C/3270°F. Firecrete 97 has a very high strength and abrasion resistance. Used for general application in severe conditions. Recommended for special atmospheres, particularly resistant to chemical attack in the ammonia production processes where hydrogen atmospheres are encountered.

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramic
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 2.85 g/cc0.103 lb/in³dried to 110°C
Grain Size <= 7000 µm<= 7000 µm
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 37.3 MPa5410 psiCold Crushing Strength, MST
 29.4 MPa
@Treatment Temp. 1000 °C
4260 psi
@Treatment Temp. 1830 °F
Cold Crushing Strength
 30.4 MPa
@Treatment Temp. 815 °C
4410 psi
@Treatment Temp. 1500 °F
Cold Crushing Strength
 49.0 MPa
@Treatment Temp. 110 °C
7110 psi
@Treatment Temp. 230 °F
Cold Crushing Strength
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  1.80 W/m-K
@Temperature 1200 °C
12.5 BTU-in/hr-ft²-°F
@Temperature 2190 °F
 1.84 W/m-K
@Temperature 1000 °C
12.8 BTU-in/hr-ft²-°F
@Temperature 1830 °F
 1.85 W/m-K
@Temperature 800 °C
12.8 BTU-in/hr-ft²-°F
@Temperature 1470 °F
 1.89 W/m-K
@Temperature 600 °C
13.1 BTU-in/hr-ft²-°F
@Temperature 1110 °F
Maximum Service Temperature, Air <= 1800 °C<= 3270 °F
Shrinkage 0.10 %0.10 %MST
 0.10 %
@Treatment Temp. 815 °C
0.10 %
@Treatment Temp. 1500 °F
 0.20 %
@Treatment Temp. 1000 °C
0.20 %
@Treatment Temp. 1830 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 96.3 %96.3 %
CaO 2.5 %2.5 %
Fe2O3 0.10 %0.10 %
K2O+Na2O >= 0.50 %>= 0.50 %
SiO2 >= 0.10 %>= 0.10 %
 
Descriptive Properties
Net Material Required (kg/m³)2780
Water Addition[8% by weight]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Bismuth Alloy
Overview of materials for Acetal Copolymer, Carbon Fiber Filled

CMORF6049 / 202833

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.