MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M SJ6344 Protective Product, Molded Shapes
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: 3M Bumpon Protective Products SJ6344 is a pressure-sensitive adhesive-backed, molded polyurethane product. The Bumpon SJ6344 is called an Easy Slide Series because it incorporates a special abrasion resistant film in its construction, allowing the Bumpon to be used as a lower friction foot, for heavier product applications. Bumpon SJ6344 has a reduced coefficient of friction compared to our standard line of molded or rollstock version Bumpon products. In customer applications where protective anti-skid feet are preferred for heavier electronic or desktop items, but allows some sliding, it provides a unique solution. In cases where items would normally require lifting, it often allows it to be pushed or pulled slowly across a uniform surface.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore M 7272ASTM D2240
Coefficient of Friction, Dynamic 0.200.20Glass; ASTM D1894
 0.200.20Wood; ASTM D1894
 0.300.30Stainless Steel; ASTM D1894
 0.300.30Formica laminate; ASTM D1894
Peel Strength 9.12 kN/m52.0 pli90°, Adhesion to Polypropylene
 9.64 kN/m55.0 pli90°, Adhesion to Polystyrene
 9.64 kN/m55.0 pli90°, Adhesion to ABS
 9.64 kN/m55.0 pli90°, Adhesion to Stainless Steel
 9.64 kN/m55.0 pli90°, Adhesion to Aluminum
Taber Abrasion, mg/1000 Cycles 0.0200.020H18, 1 kg; ASTM C501
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 66.0 °C151 °F
 107 °C225 °FIntermittent
Minimum Service Temperature, Air -34.0 °C-29.2 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature >= 5.00 °C>= 41.0 °FApplication
 <= 52.0 °C<= 126 °FApplication
 
Descriptive Properties
Adhesive TypeR-25 Synthetic Rubber
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aearo E-A-R Specialty Composites Isoloss® HD Polyurethane Elastomer
3M SJ5000 Protective Product, Molded Shapes
NRI Syntho-plug™
ITW Devcon Flexane® Rubber Repair / Castable Urethane High Performance Putty, Black
ITW Devcon Flexane® Rubber Repair / Castable Urethane 94 Liquid, Black

PMM35260 / 170007

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.