MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Aperam Supermimphy® T Cold Rolled Strip
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: SUPERMIMPHY T is nickel-iron soft magnetic alloy with very high permeability and high purity suitable for toroidal cores (e.g. wound strip used in Earth Leakage Circuit Breakers) and high performance current transformer cores

International standards: DIN 17405, IEC 404, JIS C 2531

Information provided by Aperam

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.70 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 320Hard Temper
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.000060 ohm-cm
Magnetic Permeability 315000
@Thickness 0.0700 mm,
Frequency 60 Hz
at 5 mOe, DC
 <= 430000
@Thickness 0.0700 mm,
Frequency 60 Hz
AC
Curie Temperature 420 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.0 µm/m-°C
Specific Heat Capacity 0.460 J/g-°C
Thermal Conductivity 19.0 W/m-K
Melting Point 1450 °C
 
Component Elements PropertiesOriginal ValueComments
Iron, Fe 15 %
Molybdenum, Mo 5.0 %
Nickel, Ni 80 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Touchstone CFOAM® 25 Structural Carbon Foam
NanoAmor 95%, OD/ID: 20-40/5-10 nm Aligned Multi-Walled Carbon Nanotubes
Honeywell PTM3180 Phase Change Thermal Interface Material
Honeywell PTM1300-SP
General Plastics LAST-A-FOAM® FR-3840 FST Polyurethane Foam

NPERA011 / 194800

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.