MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
EMS-Grivory Grivory® XE 5106 (GVL-4H V0) PA*-GF40
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Product description: Grivory XE 5106 black 9915 is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide. The product is flame retarded and reinforced by 40% long glass fibers. Grivory XE 5106 black 9915 is characterized by the following key-properties:
  • flame retardancy of V-0 and 5VA at 1.6 mm
  • Glow wire ignition > 800°C, CTI 600 V
  • very high stiffness and strength even after conditioning and over a wide temperature range
  • excellent notched impact resistance also at low temperatures
  • very low creep
  • high heat distortion temperatures
  • low moisture absorptionvery good dimensional stability and little warpageGrivory XE 5106 is halogen free and does not contain red phosphorus. It complies with the regulations acc. RoHS (2002/95/EC) and is not affected by the guideline 2002/96/EC (WEEE) for Electro-Appliances. The product has been designed for injection molding of technical parts especially in the area of flame retardant parts with no electrostatic charging possible Grivory XE 5106 (GVL-4H V0) black 9915 is used in the following market segments:
    • automotive
    • mechanical engineering
    • electro-mechanical parts
    The glass fibers are aligned in parallel and are just as long as the pellets (usually 10 mm).

    Information provided by EMS Grivory

  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 1.50 g/ccDry; ISO 1183
    Water Absorption 4.1 %Sim. to ISO 62
    Moisture Absorption 1.10 %Sim. to ISO 62
    Linear Mold Shrinkage, Flow 0.0010 cm/cmISO 294-4, 2577
    Linear Mold Shrinkage, Transverse 0.0030 cm/cmISO 294-4, 2577
     
    Mechanical PropertiesOriginal ValueComments
    Ball Indentation Hardness 250 MPaConditioned; ISO 2039-1
     265 MPaDry; ISO 2039-1
    Tensile Strength at Break 175 MPaConditioned; ISO 527-1/-2
     200 MPaDry; ISO 527-1/-2
    Elongation at Break 2.1 %Dry; ISO 527-1/-2
     2.4 %Conditioned; ISO 527-1/-2
    Tensile Modulus 13000 MPaConditioned; ISO 527-1/-2
     14500 MPaDry; ISO 527-1/-2
    Charpy Impact Unnotched 65.0 kJ/m²
    @Temperature 23.0 °C
    Conditioned; ISO 179/1eU
     70.0 kJ/m²
    @Temperature 23.0 °C
    Dry; ISO 179/1eU
     70.0 kJ/m²
    @Temperature -30.0 °C
    Dry; ISO 179/1eU
     70.0 kJ/m²
    @Temperature -30.0 °C
    Conditioned; ISO 179/1eU
    Charpy Impact, Notched 25.0 kJ/m²
    @Temperature 23.0 °C
    Dry; ISO 179/1eA
     25.0 kJ/m²
    @Temperature -30.0 °C
    Dry; ISO 179/1eA
     25.0 kJ/m²
    @Temperature 23.0 °C
    Conditioned; ISO 179/1eA
     25.0 kJ/m²
    @Temperature -30.0 °C
    Conditioned; ISO 179/1eA
     
    Electrical PropertiesOriginal ValueComments
    Volume Resistivity 1.00e+10 ohm-cmDry; IEC 60093
     1.00e+10 ohm-cmConditioned; IEC 60093
    Surface Resistance 1.00e+11 ohmIEC 60093
    Dielectric Strength 33.0 kV/mmDry; IEC 60243-1
     33.0 kV/mmConditioned; IEC 60243-1
    Comparative Tracking Index 600 VConditioned; IEC 60112
     
    Thermal PropertiesOriginal ValueComments
    CTE, linear, Parallel to Flow 20.0 µm/m-°CISO 11359-1/-2
    CTE, linear, Transverse to Flow 50.0 µm/m-°CISO 11359-1/-2
    Melting Point 260 °C10°C/min; ISO 11357-1/-3
    Maximum Service Temperature, Air 100 - 120 °CLong Term; ISO 2578
     220 °CShort Term; EMS
    Deflection Temperature at 1.8 MPa (264 psi) 250 °CISO 75-1/-2
    Deflection Temperature at 8.0 MPa 210 °CISO 75-1/-2
    Flammability, UL94 V-0IEC 60695-11-10
     5VAIEC 60695-11-20
     
    Descriptive Properties
    AutomotiveAutomotive electr. and electronics, lighting
     Cooling and climate control
     Exterior
     Interior
     Powertrain and Chassis
    Electricals & ElectronicsConnectors
     Electrical appliances
     Electrical equipment
     Energy distribution
     Lighting
    FormGranules
    Industry & Consumer goodsHeating systems
     Housewares
     Hydraulics & Pneumatics
     Mechanical Engineering
     Power transmission
     Sports & Leisure
     Tools & Accessories
    ProcessingInjection Molding
    Product AttributesLong Fiber Reinforced
     Partially aromatic Polyamide
    Special CharacteristicsFlame retardant
     Improved heat resistance

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Celanese Zytel® HTN51G35HSL NC010 PA6T/XT-GF35
    Celanese FORTRON 1140L6 PPS, 40% Glass Reinforced
    Celanese FORTRON 1130L4 PPS, 30% Glass Reinforced
    Celanese VECTRA E115i LCP, 15% Glass Reinforced
    Celanese Thermx® CG933 NC010 PCT

    PGRH414 / 157123

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.