MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Solvay FM® 73M Epoxy Film Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: FM® 73 film adhesive is a toughened, general purpose aerospace epoxy designed to provide excellent structural performance from -67°F to 180°F (-55°C to 82°C). FM 73 film adhesive is formulated to provide outstanding durability in bonding metals and is also suitable for boding many structural composite systems. Extensive testing has proven that FM 73 adhesive meets stringent environmental resistance and bonding durability requirements. To achieve maximum environmental resistance and bonding durability the use of BR® 127 corrosion inhibiting primer is recommended in bonding metallic components.

Features & Benefits:

  • Demonstrates excellent peel strength and structural performance from -67°F to 180°F (-55°C to 82°C)
  • Resistant to pre-bond humidity exposure
  • Good moisture and corrosion resistance in high humidity
  • Shop life of 15 days at 75°F (24°C)
Applications:
  • Metal-to-metal bonding
  • Composite-to-composite bonding
  • Composite-to-metal bonding

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 1.25 %
Outgassing - Total Mass Loss 0.78 %TWL
Collected Volatile Condensable Material 0.00 %
Storage Temperature <= -18.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 720 psi
@Temperature 82.0 °C
Flatwise, 0.06 lb/ft2
 830 psi
@Temperature 82.0 °C
Flatwise, 0.085 lb/ft2
 1050 psi
@Temperature 24.0 °C
Flatwise, 0.06 lb/ft2
 1450 psi
@Temperature 24.0 °C
Flatwise, 0.085 lb/ft2
 1500 psi
@Temperature -55.0 °C
Flatwise, 0.06 lb/ft2
 1580 psi
@Temperature -55.0 °C
Flatwise, 0.085 lb/ft2
Shear Strength 4770 psi0.03 lb/ft2, 7 days immersion in hydrocarbon fluid (TT-S-735)
 4780 psi0.03 lb/ft2, 30 days salt spray
 4790 psi0.03 lb/ft2, 30 days salt spray
 4880 psi0.03 lb/ft2, 7 days immersion in JP-4 fuel (MIL-J-5624)
 4930 psi0.06 lb/ft2, 30 days salt spray
 4960 psi0.03 lb/ft2, 30 days at 120°F (50°C) and 95 – 100% R.H.
 4980 psi0.06 lb/ft2, 30 days salt spray
 4990 psi0.06 lb/ft2, 30 days at 120°F (50°C) and 95 – 100% R.H.
 5040 psi0.06 lb/ft2, 7 days immersion in JP-4 fuel (MIL-J-5624)
 5060 psi0.06 lb/ft2, 7 days immersion in hydrocarbon fluid (TT-S-735)
 3650 psi
@Temperature 82.0 °C
Blister, Metal-to-Metal, 0.03 lb/ft2
 4050 psi
@Temperature 82.0 °C
Metal-to-Metal, 0.03 lb/ft2
 4860 psi
@Temperature 24.0 °C
Blister, Metal-to-Metal, 0.03 lb/ft2
 5290 psi
@Temperature -55.0 °C
Blister, Metal-to-Metal, 0.03 lb/ft2
 5770 psi
@Temperature 24.0 °C
Metal-to-Metal, 0.03 lb/ft2
 5890 psi
@Temperature -55.0 °C
Metal-to-Metal, 0.03 lb/ft2
Peel Strength 55.0 pli
@Temperature 82.0 °C
Floating Roller metal-to-metal, 0.03 lb/ft2; ASTM D3167-76
 56.0 pli
@Temperature -55.0 °C
Floating Roller metal-to-metal, 0.03 lb/ft2; ASTM D3167-76
 64.0 pli
@Temperature 24.0 °C
Floating Roller metal-to-metal, 0.03 lb/ft2; ASTM D3167-76
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 82.0 °C
Minimum Service Temperature, Air -55.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
ColorDark Green0.13 mm
 Yellow0.18 mm
 Yellow0.25 mm
 Yellow0.38 mm
Metal-to-Metal Climbing Drum Peel220 Nm/m-55°C, 0.03 lb/ft2, ASTM D1781-76
 290 Nm/m24°C, 0.03 lb/ft2, ASTM D1781-76
 300 Nm/m-55°C, 0.06 lb/ft2, ASTM D1781-76
 380 Nm/m82°C, 0.03 lb/ft2, ASTM D1781-76
 390 Nm/m24°C, 0.06 lb/ft2, ASTM D1781-76
 570 Nm/m82°C, 0.06 lb/ft2, ASTM D1781-76
Sandwich Peel100 Nm/m-55°C, 0.085 lb/ft2
 130 Nm/m24°C, 0.06 lb/ft2
 180 Nm/m24°C, 0.085 lb/ft2
 56 Nm/m82°C, 0.06 lb/ft2
 59 Nm/m82°C, 0.085 lb/ft2
 74 Nm/m-55°C, 0.06 lb/ft2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay FM® 73 Epoxy Film Adhesive
Henkel Hysol EA 9330 Paste Adhesive System
Henkel Hysol EA 9313 Paste Adhesive System
Solvay FM® 300M Epoxy Film Adhesive
Solvay FM® 300 Epoxy Film Adhesive

PCYTED047 / 180349

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.