Description: AKROTEK® PEEK GF 50 9 natural (5183) is a 50 % glass fibre reinforced process improved polyetheretherketone with very high stiffness and strength Applications: Applications are mainly elements in the automotive-, aeronautical-, industrial- and medical engineering that require high strength in a temperature environment above 150 °C Information provided by Akro-Plastic GmbH |