MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Firemaster® Putty Putty
Categories: Ceramic; Oxide; Other Engineering Material

Material Notes: FireMaster® putty is composed of Superwool ® HT, a low biopersistent fiber, organic polymers, inorganic binders and other proprietary ingredients. FireMaster® putty is a pliable, low shrinkage, putty-like material that is supplied wet and premixed, ready for installation by a pneumatically applied system for large areas or hand trowelling for typical Firestop applications. FireMaster® putty is Underwriters Laboratory tested and listed as a Firestop sealant per ASTM E814 (UL1479) in multiple Firestop designs for up to 3 hour F and T- Ratings. UL Follow-Up Service audits provide assurance that the product supplied to the job sites meets the same tight quality standards as the materials supplied for fire testing.

Information provided by Morgan Advanced Materials

Key Words: Putty
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.120 g/ccwet, as received
 0.513 - 0.577 g/cc
@Temperature 110 °C
dried
Solids Content 46 %
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air <= 1482 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Component Elements PropertiesOriginal ValueComments
CaO 12 %
Other 2.0 %
SiO2 86 %
 
Descriptive Properties
Coloraluminum gray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CMORF6140 / 202924

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.