MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
3M Scotchkote™ XF 895 Fast Curing Floor Coating
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Liquid

Material Notes: Scotchkote Fast Curing Floor Coating XF 895 has been specifically developed as a high build floor protection system for application to concrete surfaces, to provide rapid return to service

Product Features:

  • Combines good application characteristics with excellent adhesion to concrete
  • Designed for application by brush or roller
  • Suitable for return to service in 1.5 hrs
  • Also suitable for use on asphalt floor surfaces in combination with 3M Scotchkote Primer FB 856

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/cc
Solids Content 100 %
Thickness 6.00 - 8.00 mil
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 75 - 80ASTM D2240
Tensile Strength at Break 22.6 MPaASTM D638
Elongation at Break 15 - 20 %ASTM D412
Abrasion 78[mg] 1000 cycles
 
Processing PropertiesOriginal ValueComments
Cure Time 0.750 - 1.00 hourTouch Dry
 1.00 - 1.50 hourHard Dry
 168 hourFull Cure
 
Descriptive Properties
AppearanceLight Gray, Clear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMM35316 / 170063

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.