MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC VALOX™ FR 771 PBT (Americas)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: VALOX 771 is a 35% mineral/glass filled, flame retardant Polybutylene Terephthalate (PBT) injection moldable grade. It has excellent chemical resistance and a UL94V0@0.75 flame rating and 5VA@2.0mm. This grade also has a CTI of 0 and is a good candidate for applications that may see electrical arcing.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.70 g/cc1.70 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0065 - 0.0085 cm/cm0.0065 - 0.0085 in/inSABIC method
Linear Mold Shrinkage, Transverse 0.010 - 0.012 cm/cm0.010 - 0.012 in/inSABIC method
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 72.0 MPa10400 psi5 mm/min; ASTM D638
Elongation at Break 2.3 %2.3 %5 mm/min; ASTM D638
Flexural Strength 110 MPa16000 psibrk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 5.86 GPa850 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.420 J/cm0.787 ft-lb/inASTM D256
Izod Impact, Unnotched 3.90 J/cm7.31 ft-lb/inASTM D4812
 
Electrical PropertiesMetricEnglishComments
Arc Resistance 180 - 240 sec180 - 240 secASTM D495
Comparative Tracking Index >= 600 V>= 600 VUL 746A
Hot Wire Ignition, HWI >= 120 sec>= 120 secUL 746A
High Amp Arc Ignition, HAI >= 120 arcs>= 120 arcsUL 746A
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min0.000 - 0.394 in/minUL 746A
 
Thermal PropertiesMetricEnglishComments
Hot Ball Pressure Test 125 °C257 °FIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 217 °C
@Thickness 6.40 mm
423 °F
@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 196 °C
@Thickness 6.40 mm
385 °F
@Thickness 0.252 in
unannealed; ASTM D648
UL RTI, Electrical 140 °C284 °FUL 746B
UL RTI, Mechanical with Impact 125 °C257 °FUL 746B
UL RTI, Mechanical without Impact 140 °C284 °FUL 746B
Flammability, UL94  V-2
@Thickness 0.610 mm
V-2
@Thickness 0.0240 in
UL 94
 V-0
@Thickness 0.760 mm
V-0
@Thickness 0.0299 in
UL 94
 5VA
@Thickness 2.01 mm
5VA
@Thickness 0.0791 in
UL 94
Glow Wire Test  750 °C
@Thickness 1.00 mm
1380 °F
@Thickness 0.0394 in
IEC 60695-2-13
 800 °C
@Thickness 3.00 mm
1470 °F
@Thickness 0.118 in
IEC 60695-2-13
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
IEC 60695-2-12
 960 °C
@Thickness 1.00 mm
1760 °F
@Thickness 0.0394 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 255 - 270 °C491 - 518 °FInjection Molding
Zone 1 245 - 255 °C473 - 491 °F
Zone 2 250 - 260 °C482 - 500 °F
Zone 3 255 - 265 °C491 - 509 °F
Melt Temperature 255 - 275 °C491 - 527 °F
Mold Temperature 65.0 - 95.0 °C149 - 203 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 12.0 hour12.0 hourCumulative; Injection Molding
Moisture Content 0.020 %0.020 %
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 40 - 80 %40 - 80 %
Vent Depth 0.00250 - 0.00380 cm0.000984 - 0.00150 in
Screw Speed 50 - 80 rpm50 - 80 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI10321 / 243788

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.