MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Celanese Celanex® 3316CT PBT, 50% Glass Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled

Material Notes: Celanex 3316CT is a non-exuding, 50% glass/min, flame retarded PBT, which has an excellent balance of mechanical properties and processability. Celanex 3316CT is specifically designed to exhibit very high CTI.

Information provided by Celanese Corporation.

Key Words: High CTI, flame retarded PBT
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.81 g/cc1.81 g/ccASTM D792
Density 1.81 g/cc0.0654 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0020 - 0.0030 cm/cm0.0020 - 0.0030 in/inISO 294-4
 0.0020 - 0.0040 cm/cm0.0020 - 0.0040 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0055 - 0.0075 cm/cm0.0055 - 0.0075 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 84.0 MPa12200 psi5mm/min; ISO 527-2/1A
 82.0 MPa
@Temperature 22.8 °C
11900 psi
@Temperature 73.0 °F
ASTM D638
Elongation at Break 1.5 %1.5 %5mm/min; ISO 527-2/1A
Tensile Modulus 11.0 GPa1600 ksi1mm/min; ISO 527-2/1A
Flexural Strength 135 MPa19600 psiISO 178
 134 MPa
@Temperature 22.8 °C
19500 psi
@Temperature 73.0 °F
ASTM D790
Flexural Modulus 10.775 GPa1562.8 ksiISO 178
 11.33 GPa
@Temperature 22.8 °C
1643 ksi
@Temperature 73.0 °F
ASTM D790
Izod Impact, Notched 0.694 J/cm
@Temperature 22.8 °C
1.30 ft-lb/in
@Temperature 73.0 °F
ASTM D256
Izod Impact, Notched (ISO) 8.00 kJ/m²3.81 ft-lb/in²ISO 180/1A
Izod Impact, Unnotched (ISO) 33.0 kJ/m²
@Temperature 23.0 °C
15.7 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1U
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmASTM D257
Dielectric Strength 26.0 kV/mm660 kV/inshort term; ASTM D149
Arc Resistance 136 sec136 secASTM D495
Comparative Tracking Index 600 V600 VASTM D3638
 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 222 °C432 °FISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 201 °C394 °FISO 75-1, -2
Flammability, UL94 V-0V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Rynite® 530HTE NC010 PET-GF30
Celanese Rynite® 530 NC010 PET-GF30
DuPont Mobility and Materials Rynite® FR530L BK507 Polyethylene Terephthalate (PET)
Celanese Celanex® XFR 6842 GF20 PBT, 30% Glass Reinforced
Celanese Celanex® 2014 Flame Retarded Unreinforced Polybutylene Terephthalate

PHCS060 / 123475

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.