MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Solvay MIRACARE® BC-20 Surfactant  (discontinued **)
Categories: Fluid

Material Notes: Description: MIRACARE BC-20 is a concentrated baby shampoo formula which yields a finished product upon dilution. MIRACARE BC-20 retains the traditional ultra-mild shampoo ingredients, while combining with additional “hair softening” agents

Chemical Name: SURFACTANT BLEND

CAS: 7732-16-5; 68154-33-6; 70851-07-9; 25446-78-0; 56-81-5; 68608-66-2; 9005-08-7; 33939-64-9; 50546-32-2; 33939-65-0

I.N.C.I.: Water (and) PEG-80 Sorbitan Laurate (and) Cocamidopropyl Betaine (and) Sodium Trideceth Sulfate (and) Glycerin (and) Sodium Lauroamphoacetate (and) PEG-150 Distearate (and) Sodium Laureth-13 Carboxylate

Available in: Asia Pacific, Europe, Latin America and North America

Applications: MIRACARE® BC-20 is a concentrated baby shampoo formula which yields a finished product upon dilution. MIRACARE® BC-20 retains the traditional ultra-mild shampoo ingredients, while combining with additional “hair softening” agents

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/cc
Solids Content 42 - 46 %Microwave; RP-0531
pH 7.5 - 8.5RP-0420
Viscosity <= 5000 cP#4 SP @ 20 rpm; RP-0659
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 6.0RP-0138
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceClear LiquidRP-0064
CompositionMicrobial Contam.< 1 cfu/mL, Petrifilm Method, RP-0659
 Total Non Volatiles16-18%

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 1137 Steel, cold drawn, low temperature, stress relieved, round
AISI 1040 Steel, as cold drawn, 16-22 mm (0.625-0.875 in) round
AISI 1030 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round

WRHOD234 / 137465

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.