MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Cookson Group STAYSTIK® Resin E Patented Technology Paste  (discontinued **)
Categories: Polymer; Adhesive; Thermoplastic

Material Notes: This thermoplastic adhesive paste is a solvent based polymer specially developed for temporary bonding applications most typically associated with tape head slider manufacturing but can be used for a variety of applications were temporary adhesion is necessary. This adhesive is commonly debonded in NMP leaving no residue or contamination on the surface of the debonded assembly.

Applications:

  • Wafer lapping
  • Substrate cutting
  • Wafer cutting
  • Wafer polishing
  • Row bonding for dicing
  • Lens polishing

Information provided by Cookson Electronics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Adhesive Bond Strength >= 2500 psi
 
Processing PropertiesOriginal ValueComments
Drying Temperature 70.0 °CFor 10 minutes, Open face
 
Descriptive Properties
Attach Temperature100-140°C
Dwell Time5-25 seconds
Pressure During Dwell Time0-5 psi

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPLASK057 / 56347

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.