MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polytek PlatSilĀ® SiliGlass Silicone Rubber
Categories: Polymer; Thermoset; Silicone

Material Notes: PlatSil SiliGlass is a platinum-cured silicone designed for making super-clear, glass-like rubber castings for special effects and prop applications. SiliGlass is designed to act and look like broken glass when hit. Since the broken glass-like shards are made of a safe silicone rubber, there is no danger to an actor or actress during its use.

Information provided by Polytek

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.970 g/cc
Viscosity 200 cPMixed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 40
 
Processing PropertiesOriginal ValueComments
Cure Time 0.500 hourDemold Time
 7.00 minPour Time
 24.0 hourTotal Cure
 
Descriptive Properties
Cured ColorClear
Mix Ratio By Weight1A:1B
Part A ColorClear
Part B ColorClear
Specific Volume28 in3/lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPTK5010 / 251002

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.