MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis Fibremod™ GD302HP Polypropylene, Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Glass Fiber Filler

Material Notes: GD302HP is a 30% chemically coupled high performance glass fiber reinforced polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process. Applications: dashboard carriers, door module carriers, and structural seat parts.

Former trade name for this product was Xmod™.

Information provided by Borealis AG

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.00060 cm/cm0.00060 in/inaverage process; 150x80x2mm
Linear Mold Shrinkage, Transverse 0.00080 cm/cm0.00080 in/inaverage process; 150x80x2mm
Melt Flow 3.3 g/10 min
@Load 2.16 kg,
Temperature 230 °C
3.3 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 65.0 MPa9430 psiISO 527-2
Elongation at Yield 4.0 %4.0 %ISO 527-2
Tensile Modulus 5.60 GPa812 ksi1mm/min; ISO 527-2
Flexural Strength 86.0 MPa12500 psiISO 178
Flexural Modulus 5.10 GPa740 ksi2mm/min; ISO 178
Izod Impact, Notched (ISO)  16.0 kJ/m²
@Temperature -20.0 °C
7.61 ft-lb/in²
@Temperature -4.00 °F
ISO 180/1A
 28.0 kJ/m²
@Temperature 23.0 °C
13.3 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched  6.00 J/cm²
@Temperature -20.0 °C
28.6 ft-lb/in²
@Temperature -4.00 °F
ISO 179/1eU
 6.50 J/cm²
@Temperature 23.0 °C
30.9 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  1.30 J/cm²
@Temperature -30.0 °C
6.19 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 2.40 J/cm²
@Temperature 23.0 °C
11.4 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 132 °C270 °FISO 75-2
 
Processing PropertiesMetricEnglishComments
Feed Temperature 40.0 - 80.0 °C104 - 176 °F
Melt Temperature 230 - 280 °C446 - 536 °Fmass temperature
Mold Temperature 30.0 - 50.0 °C86.0 - 122 °F
Injection Velocity 100 - 200 mm/sec3.94 - 7.87 in/sec
Hold Pressure 30.0 - 60.0 MPa4350 - 8700 psi
 
Descriptive Properties
Back Pressureas low as possible
Screw Speedlow to medium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis KSR4525 Polypropylene Reactor Elastomer Modified
Adell RR-16 Copolymer Polypropylene, 30% Glass Reinforced
Borealis Fibremod™ GB306SAF Polypropylene, Glass Fiber Reinforced
Borealis Fibremod™ GB364WG Polypropylene Compound, Glass Fiber Reinforced
Borealis Fibremod™ GD301FE Polypropylene, Glass Fiber Reinforced

PBOREA611 / 108870

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.