MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman INVISION™ VX-5075UI Soft Touch Polyolefin Thermoplastic
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Description

Invision™ VX-5075UI is a polyolefin-based thermoplastic of 75 Shore A durometer, which has been formulated for soft touch, mar resistance, low gloss, and excellent weatherability.
Application

Invision™ VX-5075UI is targeted for automotive injection molding appearance applications.
Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.880 g/cc0.880 g/ccISO 1183/1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 767615 sec delay; ISO 868
Tensile Strength at Break 5.80 MPa841 psiISO 527
Tensile Stress at Strain 3.60 MPa
@Strain 100 %
522 psi
@Strain 100 %
ISO 527
Elongation at Break >= 350 %>= 350 %ISO 527
Tear Strength 34.0 kN/m194 pliISO 34/1
 
Descriptive Properties
Colorfastness/Weatherability 1240 Delta E (kJ/m^2)SAE J1885
Fogging0.9SAE J1756, 95°C, Dry Fog

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Isoflon PTFE +28% GL Blue-E glass-1% Blue Polytetrafluoroethylene with 28% GL-Blue-E glass-1% Blue (equivalent VX1)
Dow AFFINITY™ EG 8200G Ethylene alpha-olefin copolymer
Dow AFFINITY™ PF 1140G Polyolefin Plastomer (POP)
Borealis Borlink™ LE0504 Crosslinkable Semiconductive Shielding Compound
Borealis Borlink™ LE0500 Crosslinkable Semiconductive Shielding Compound

PASHU055 / 25019

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.