Description: COHRlastic® CF silicone solid rubber reinforced with fiberglass is a dimensionally-stable, durable material for press pads, belting and gasketing. It is available in six constructions. CF 4032 and CF 4050 are thin, flexible and abrasion-resistant for general purpose use. GRAY in color. All data based on a 0.03125 inch test sample.(Tolerance of .005"; Thickness shown is for silicone rubber. Fiberglass thickness = 0.014".) Information provided by Saint Gobain Performance Products. |