MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Baydur® 660 IBS Polyurethane Structural Foam RIM, Density 40 pcf, MDI-based 2-Component Liquid System  (discontinued **)
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: 0.25 in. thickness. IBS = Interactive Blowing System RIM = Reaction Injection Molding

Information provided by Bayer Corporation, Polyurethanes Division

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.640 g/cc0.0231 lb/in³ASTM D792
Apparent Bulk Density 0.640 g/cc0.0231 lb/in³ASTM D792
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm0.0030 - 0.0050 in/inBayer Test
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6767ASTM D2240
Tensile Strength, Ultimate 22.0 MPa3190 psiASTM D638/D412
Elongation at Break 7.0 %7.0 %ASTM D638/D412
Flexural Yield Strength 26.0 MPa3770 psiASTM D790
Flexural Modulus 1.21 GPa175 ksiASTM D790
Compressive Yield Strength 31.0 MPa4500 psiASTM D395
Charpy Impact, Notched 1.40 J/cm²6.66 ft-lb/in²Bayer Test
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C185 °FASTM D648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Baydur® 646 Polyurethane Structural Foam RIM, Density 15 pcf, MDI-based 2-Component Liquid System
Covestro Baydur® 646 Polyurethane Structural Foam RIM, Density 20 pcf, MDI-based 2-Component Liquid System
Covestro Baydur® 646 Polyurethane Structural Foam RIM, Density 25 pcf, MDI-based 2-Component Liquid System
Covestro Baydur® 660 IBS Polyurethane Structural Foam RIM, Density 30 pcf, MDI-based 2-Component Liquid System
Covestro Baydur® STR/F-275 IMR Polyurethane Composite SRIM Foam, 20% Glass Filled, MDI-based 2-Component Liquid System

PB2B04 / 26579

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.