Product Description: A super white opaque, high gloss, high yield and highly cavitated BOPP film designed for use in reel-fed wrap-around labeling applications where superior graphics are desired. Availability: Africa & Middle East, Asia Pacific and Europe Key Features: - Outstanding opacity and whiteness
- Exceptional printability
- Excellent hot melt anchorage
- Excellent stiffness
- High tear and split resistance
- High resistance to elongation on labeling machine
- Good mold resistance
- High slip on untreated side of 38DL247 for optimized performance on the most demanding machines
Applications:- Beverage, Alcoholic
- Beverage, Carbonated
- Beverage, Mineral Waters
- Dairy Products
- Health and Beauty Care
- Household and Detergents
- Industrial
Uses: Processing Method: Inner Web Adhesion Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing, Surface Print Unsupported, UV Flexographic Printing and UV Offset Lithography PrintingInformation provided by ExxonMobil |