MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Henkel Loctite® Stycast® 2651-40 W1 with CAT 9 Epoxy Encapsulant
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Loctite Stycast 2651-40 W1 provides the following product characteristics:
  • Low viscosity
  • Room temperature cure capability
  • Can be color coded to specification

Cure: Room temperature or Heat cure

Application: Potting, Encapsulant

Loctite Stycast 2651-40 W1 epoxy encapsulant is designed for general purpose applications and has excellent adhesion to a wide variety of substrates. When fully cured, the material is readily machined with carbide tools.

Loctite Stycast 2651-40 W1 can be used with a variety of catalysts.

CATALYST DESCRIPTION

Loctite CAT 9 provides the following product characteristics:

  • General purpose
  • Good chemical resistance
  • Good physical strength

Cure: Room temperature cure

Information provided by Henkel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³Part B, Loctite CAT 9
 1.50 g/cc0.0542 lb/in³Part A, Loctite Stycast 2651-40 W1
Water Absorption  0.030 %
@Time 86400 sec
0.030 %
@Time 24.0 hour
Cured
 0.070 %
@Time 605000 sec
0.070 %
@Time 168 hour
7 Days, Cured
Viscosity 450 cP450 cPPart B, Loctite CAT 9
Brookfield Viscosity 33000 cP33000 cPPart A, Loctite Stycast 2651-40 W1; Spindle 6, speed 5 rpm
Linear Mold Shrinkage 0.0050 cm/cm0.0050 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9090
Modulus of Elasticity  0.101 GPa
@Temperature 150 °C
14.6 ksi
@Temperature 302 °F
 0.726 GPa
@Temperature 100 °C
105 ksi
@Temperature 212 °F
 4.361 GPa
@Temperature 50.0 °C
632.5 ksi
@Temperature 122 °F
 4.463 GPa
@Temperature 35.0 °C
647.3 ksi
@Temperature 95.0 °F
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.40e+15 ohm-cm1.40e+15 ohm-cm
Surface Resistance 6.60e+15 ohm6.60e+15 ohm
Dielectric Constant  3.9
@Frequency 1e+6 Hz
3.9
@Frequency 1e+6 Hz
 4.6
@Frequency 1000 Hz
4.6
@Frequency 1000 Hz
 4.8
@Frequency 50 Hz
4.8
@Frequency 50 Hz
Dissipation Factor  0.030
@Frequency 1e+6 Hz
0.030
@Frequency 1e+6 Hz
 0.044
@Frequency 1000 Hz
0.044
@Frequency 1000 Hz
 0.052
@Frequency 50 Hz
0.052
@Frequency 50 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 60.0 µm/m-°C33.3 µin/in-°FBelow Tg
 148 µm/m-°C82.2 µin/in-°FAbove Tg
Thermal Conductivity 0.480 W/m-K3.33 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 130 °C266 °FContinuous
 150 °C302 °FIntermittent
Minimum Service Temperature, Air -40.0 °C-40.0 °FContinuous
 -40.0 °C-40.0 °FIntermittent
Glass Transition Temp, Tg 110 °C230 °FDMA, Tangent Delta
 117 °C243 °FTMA
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 - 120 min
@Temperature 65.0 °C
1.00 - 2.00 hour
@Temperature 149 °F
Option 3
 240 - 360 min
@Temperature 45.0 °C
4.00 - 6.00 hour
@Temperature 113 °F
Option 2
 960 - 1440 min
@Temperature 25.0 °C
16.0 - 24.0 hour
@Temperature 77.0 °F
Option 1
Working Life 45.0 min
@Temperature 25.0 °C
45.0 min
@Temperature 77.0 °F
100 g
Shelf Life 12.0 Month12.0 MonthPart A, Loctite Stycast 2651-40 W1
 
Descriptive Properties
AppearanceBlackPart A, Loctite Stycast 2651-40 W1
Mix Ratio, by Volume100 : 13.5Material : Catalyst
Mix Ratio, by Weight100 : 9Material : Catalyst
Weight Loss (%)0.04@ 150°C
 0.1@ 200°C
 0.21@ 250°C
 0.38@ 300°C
 58.6@ 700°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHENK7917 / 255404

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.