Product Description: Accelerator EZ is a very active non-discoloring, non-staining accelerator for NR and Synthetic Rubber. It is also used for latex work. It is active in latex without zinc oxide. EZ can be used in dry rubber applications as an activator for the thiazoles. It is approximately 15% less active than Accelerator MZ without the health hazards associated with MZ. EZ is FDA listed under 177.2600 regulations.Information provided by Akrochem Corporation |