MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
AdvanSix Aegis® CSD High Barrier Nylon  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Description: Aegis CSD provides delamination resistance during production and a significantly improved, high level of passive CO2 barrier compared with monolayer PET.

Former Honeywell product; AdvanSix is a spin-off of Honeywell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.15 g/cc
Oxygen Transmission 0.600 cc-mil/100 in²-24hr-atm80% RH, 23°C, cast film
Carbon Dioxide Transmission 1.20 cc-mil/100 in²-24hr-atm80% RH, 23°C, oriented film
Melt Index of Compound 14 g/10 min
@Load 2.16 kg,
Temperature 260 °C
 24 g/10 min
@Load 2.16 kg,
Temperature 280 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 14800 psioriented film
Tensile Strength, Yield 13100 psioriented film, Yield Stress
Elongation at Break 42 %oriented film
Elongation at Yield 4.0 %oriented film
Secant Modulus 3.013 GPaoriented film
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 82.0 °CDSC method
 
Processing PropertiesOriginal ValueComments
Processing Temperature 270 - 280 °C
Feed Temperature 25.0 °C
Nozzle Temperature 280 °C
Zone 1 500 °F
Zone 2 518 °F
Zone 3 518 °F
Zone 4 527 °F
Zone 5 536 °F
Melt Temperature 233 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PALA02 / 23094

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.