Description: Peel ply. Ideally suited to aerospace applications. Features & Benefits: - Porous, nylon peel ply
- Heat set and scoured, for use directly against laminates or bond lines
- Available coated and non-coated, depending on user requirement
- Approved on a range of OEM specifications for composite manufacture and metal bonding
- This product is particularly recommended for use with phenolic resin systems
- Also recommended for composite manufacture and metal boding applications
- Manufactured by Precision Fabrics Group (PFG)
Information provided by Cytec, subsequently acquired by Solvay. |