System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Austin Novel Materials Texalan® 590A Polyether-based TPU
Categories:
Polymer
;
Thermoplastic
;
Elastomer, TPE
;
Polyurethane, TP
;
Thermoplastic Polyurethane (TPUR), Polyether Grade
Material Notes:
Good low temperature resistance,and water resistance; can be used in cold and humid temperatures.
Information from Dawnentech
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.13
-
1.17
g/cc
ISO 1183
Mechanical Properties
Original Value
Comments
Hardness, Shore A
87 - 93
ISO 7619
Tensile Strength
>=
40.0
MPa
ISO 37
Tensile Stress at Strain
>=
9.00
MPa
@Strain 100 %
ISO 37
>=
17.0
MPa
@Strain 300 %
ISO 37
Elongation at Yield
>= 500 %
ISO 37
Tear Strength
>=
105
kN/m
ISO 34
K Factor (Wear Factor)
<= 70
[mm
3
]; ISO 4649
Compression Set
<= 40 %
@Temperature 70.0 °C
ISO 815
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Covestro Texin® 5290 Thermoplastic Polyurethane, Polyether-based, Medical
Covestro Texin® 5286 Thermoplastic Polyurethane, Polyether-based, Medical
Austin Novel Materials Texalan® 295A Polyester-based TPU
Austin Novel Materials Texalan® 585A Polyether-based TPU
Austin Novel Materials Texalan® 690A Polyester and Polyether based TPU
PDAWNE032 / 123266
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.