3M™ Thermal Transfer Polyester Label Materials 7816, 7816FL and 7875 are durable polyester label stocks that offer excellent moisture resistance and thermal stability. These label products utilize 3M™ Adhesive 310 which is a firm adhesive which resists oozing and provides high strength on a variety of surfaces including high surface energy (HSE) plastics and metals.Information provided by 3M |