MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Alfa Chemistry Materials Chromium single crystal disc, (110) orientation
Categories: Metal; Nonferrous Metal; Pure Element

Material Notes: 10mm (0.39in) dia, 1-3mm (0.04-0.1in) thick, ±0.5°

Information provided by Alfa Chemistry Materials.

Vendors: Alfa Chemistry is an ISO 9001:2015 certified supplier of various materials, including: MOFs, coatings, nanomaterials, metals, polymers, carbon fibers, graphite, ceramics, glass, semiconductors, catalysts, carbon nanotubes, fullerene, COFs, molecular sieve, quantum dots, recycled plastics, photonic and optical materials, and magnetic materials, for customers worldwide. Alfa Chemistry also provides custom synthesis services for nearly all kinds of materials and chemicals. Learn more about Alfa Chemistry's high quality products at materials.alfachemic.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 7.18 g/cc
Molecular Weight 52 g/mol
 
Chemical PropertiesOriginal ValueComments
Electronegativity 1.60Paulings
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 1060MPa Microhardness
Modulus of Elasticity 279 GPa
Poissons Ratio 0.21
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000129 ohm-cm
@Temperature 0.000 °C
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 294 J/g
Heat of Vaporization 5871 J/g
CTE, linear 4.90 µm/m-°C
@Temperature 25.0 °C
Specific Heat Capacity 0.448 J/g-°C
@Temperature 25.0 °C
Thermal Conductivity 93.9 W/m-K
@Temperature 25.0 °C
Melting Point 1857 °C
Boiling Point 2672 °C
 
Descriptive Properties
Alfa Chemistry Materials CategoryMetals and Materials
AppearanceSilvery
CAS Number7440-47-3
EC Number231-157-5
MDL NumberMFCD00010944
Molecular FormulaCr
Purity99.9%, 99.99%, 99.999%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

ZZALFA0854 / 269813

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.