MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Omni Plastics OmniTech™ PMA IM UV PMMA
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Impact Modified, Molded

Material Notes: Impact modified, UV stabilized; values are based on natural or black materials unless otherwise noted.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.06 g/ccASTM D792
Linear Mold Shrinkage 0.0030 - 0.0070 in/inIsotropic; ASTM D955
Melt Flow 8.0 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 47.0 MPaASTM D638
Elongation at Break 30 %ASTM D638
Flexural Strength 59.0 MPaASTM D790
Flexural Modulus 1724 MPaASTM D790
Izod Impact, Notched 64.0 J/m
@Thickness 3.17 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 96.0 °C
@Thickness 3.17 mm
ASTM D648
Flammability, UL94 HB
@Thickness 3.17 mm
Omni Internal Testing
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 400 - 480 °F
Middle Barrel Temperature 420 - 500 °F
Front Barrel Temperature 420 - 500 °F
Nozzle Temperature 420 - 500 °F
Melt Temperature 420 - 500 °F
Mold Temperature 80.0 - 140 °F
Drying Temperature 190 °F
Dry Time <= 4.00 hour
Moisture Content <= 0.020 %
Back Pressure 50.0 - 100 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for PVC, Flexible Grade
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded
Northstar Polymers PBA-044 Polyether Curing Agent
LyondellBasell PMA Propylene glycol methyl ether acetate
INEOS Styrolution Terlux® 2812 Transparent MABS

POMNI5161 / 185307

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.