MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mitsubishi Xantar® C CM 526 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: XANTAR® C properties are: Highest flow in combination with excellent toughness. High level of purity. High stability. Bright natural color. The benefits are: easier filling of complex parts, lower mould deposit during injection molding, low volatiles level and reduced fogging tendency, better long-term property retention and improved color consistency and appearance.

Information provided by Mitsubishi Engineering Plastics Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.21 g/cc
Moisture Absorption 0.200 %
Linear Mold Shrinkage, Flow 0.0030 cm/cm
Linear Mold Shrinkage, Transverse 0.0040 cm/cm
Melt Flow 16 g/10 min
@Load 5.00 kg,
Temperature 260 °C
cm³/10 min Volumetric Rate
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 45.0 MPa
Tensile Strength, Yield 50.0 MPa
Tensile Modulus 3800 MPa
Flexural Strength 85.0 MPa
Flexural Modulus 3500 MPa
Izod Impact, Notched (ISO) 14.0 kJ/m²
@Temperature -20.0 °C
 25.0 kJ/m²
@Temperature 23.0 °C
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cm
Surface Resistance 1.00e+15 ohm
Dielectric Constant 3.0
@Frequency 1e+6 Hz
Comparative Tracking Index 250 - 400 V
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 55.0 µm/m-°C
Deflection Temperature at 1.8 MPa (264 psi) 115 °C
Vicat Softening Point 131 °C
@Load 5.10 kg
rate 50°C/h
Flammability, UL94 HB
@Thickness 1.50 mm
Oxygen Index 23 %
Glow Wire Flammability Index 750 °C
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 270 °CAs Tested; Injection
Mold Temperature 70.0 °CAs Tested; Injection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMITSU9342 / 192006

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.