MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mueller EcoStream™ C37000 Free Cutting Muntz Metal
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Mueller Brass Company’s C37000 alloy provides a viable alternative to those manufacturers who are manufacturing products and components that require compliance with the recently approved “Reduction of Lead in Drinking Water Act.” The legislation re-defines the term “lead free” to mean “… no more that a weighted average of 0.25% lead when used with respect to the wetted surfaces of pipes, plumbing fittings and fixtures.” With this in mind, Mueller Brass Company’s C37000 alloy provides a low lead alloy that aids in the compliance to this legislation, while maintaining machinability ratings and forging performance near that of conventional free cutting and forging alloys.
No Silicon • No Bismuth • No Segregation
In addition to machinability ratings near that of free cutting brass, C37000 also possesses the virtues and merits of Mueller Brass Company’s other EcoStream™ Lead Free and Low Lead alloys. Since no contaminating additives like bismuth or silicon are used in the production of this alloy, C37000 is completely recyclable with conventional brass alloys still widely being used for non-potable plumbing and industrial applications. As a result, there is no need to segregate scrap, no incurred downtime for machine clean-outs, and higher production efficiency and through-put.

Advantanges:

  • Good machinability
  • Excellent hot forgability
  • Excellent capability for brazing and plating
  • Excellent ability to thread rolled
  • Completely recyclable

Applications:

  • Screw machine parts requiring lower lead content
  • Forged parts and components in LEAD FREE applications and products

Information Provided by Mueller Industries Inc.

Key Words: ASTM B136, UNS C37000, No. 37700 (tube)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.41 g/cc0.304 lb/in³Based on UNS number
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 7878
Tensile Strength at Break 359 MPa52000 psi
Tensile Strength, Yield 138 MPa20000 psi
Elongation at Break 30 %30 %
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 59 - 62 %59 - 62 %
Iron, Fe <= 0.15 %<= 0.15 %
Lead, Pb 0.80 - 1.5 %0.80 - 1.5 %
Zinc, Zn 36.35 - 40.2 %36.35 - 40.2 %Remainder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Free-Cutting Muntz Metal, UNS C37000
Forging Brass, UNS C37700
Free-Cutting Muntz Metal, UNS C37000, H80 (Cold Drawn 25%) Temper 50 mm tube
Free-Cutting Muntz Metal, UNS C37000, O50 Temper 38 mm tube
Assab Steels 7210M Machinery Steel

NMUEL906 / 97694

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.