MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lubrizol Estane® 58252 Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: Type: Estane® 58252 is a 70A polyether-type thermoplastic polyurethane (TPU).

Features: Formulated to have one of the highest MVT values within the thermoplastic polyurethane class. It is also among the softest grades. Extruded or solution cast films of Estane 58252 TPU are non-porous and have very high moisture vapor transmission rates.

Uses: Intended for cast film and solution coating applications.

Available in Europe, Middle East, Africa, India and Asia

Information Provided by The Lubrizol Corporation

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Water Vapor Transmission 850 g/m²/day23°C, 50% RH, Water; ASTM E96B
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 70ASTM D2240
Hardness, Shore D 22ASTM D2240
Tensile Strength, Ultimate 19.3 MPaASTM D412; ASTM D638
Tensile Strength, Yield 9.00 MPa500% elongation; ASTM D412; ASTM D638
Elongation at Break 800 %ASTM D412; ASTM D638
Tensile Modulus 6.70 MPa400% elongation; ASTM D412; ASTM D638
100% Modulus 0.00280 GPa
@Strain 100 %
ASTM D412; ASTM D638
200% Modulus 0.00360 GPa
@Strain 200 %
ASTM D412; ASTM D638
300% Modulus 0.00470 GPa
@Strain 300 %
ASTM D412; ASTM D638
Tear Strength 390 pliTrouser; ASTM D470
Graves Tear Strength 270 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 140
@Load 1.00 kg
H-18 wheel; ASTM D3389-94
Tensile Set 7.0 %200% elongation; ASTM D412
 
Thermal PropertiesOriginal ValueComments
Melting Point 130 °CDSC
Vicat Softening Point 47.0 °CASTM D1525
Glass Transition Temp, Tg -28.0 °CDSC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol Estane® 58123 Thermoplastic Polyurethane
Austin Novel Materials Texalan® 598A Polyether-based TPU
Austin Novel Materials Texalan® 698A Polyester and Polyether based TPU
BASF Elastollan® S 70 A SPF TPUR
Lubrizol Estane® T365A Thermoplastic Polyurethane

PNOVEON559 / 121450

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.