MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Röchling Durostone® VEGZ-LP Vinyl Ester Composite Profile
Categories: Polymer; Thermoset; Vinyl Ester

Material Notes:

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.80 - 2.10 g/cc0.0650 - 0.0759 lb/in³ISO 1183 meth 1
Filler Content 70 - 85 %70 - 85 %glass; ISO 1172
Water Absorption <= 5.0 %<= 5.0 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 600 - 800 MPa87000 - 116000 psilongitudinal; ISO 527
Modulus of Elasticity 20.0 - 40.0 GPa2900 - 5800 ksitransverse; ISO 178
Flexural Strength 350 - 650 MPa50800 - 94300 psitransverse; ISO 178
Compressive Strength 70.0 - 150 MPa10200 - 21800 psitransverse; ISO 604
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cmIEC 60093
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 5.00 - 25.0 µm/m-°C2.78 - 13.9 µin/in-°F
Maximum Service Temperature, Air 130 °C266 °F
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PROCH9089 / 232792

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.