MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
EMS-Grivory Grivory® G 16 PA6I/6T
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Product description: Grivory G 16 is a low viscosity amorphous copolyamide. It is suitable for injection - stretch blow molding, injection blow molding, extrusion blow molding, the manufacture of coextruded blown film and mono or coex cast film and extrusion of mono- and multilayer tubes. Grivory G 16 is also used as an additive for polyamide 6 and different copolyamides to improve film properties.
  • Highly transparent and high surface gloss
  • Very good chemical resistance
  • Very good abrasion resistance
  • Excellent resistance to heat distortion
  • Excellent flavor and aroma barrier
  • Low transmission of UV-radiation
  • Improved gas and aroma barrier at elevated relative humidity
Barrier layer for mono- or co-extruded for packaging of cosmetics and foodstuffs. modifier of polyamide 6 barrier layers for flexible packaging of meat, cheese or any other foodstuff.

Information provided by EMS Grivory

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.18 g/ccDry; ISO 1183
Water Absorption 7.0 %Sim. to ISO 62
Moisture Absorption 2.00 %Sim. to ISO 62
Water Vapor Transmission 7.00 g/m²/day23°C/85% RH; ISO 15106-1/-2
Melt Flow 100 g/10 mincm³/10min Volumetric; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 85.0 MPaISO 527-3
Film Tensile Strength at Yield, TD 85.0 MPaISO 527-3
Film Elongation at Break, MD 200 %ISO 527-3
Film Elongation at Break, TD 200 %ISO 527-3
Film Elongation at Yield, MD 5.0 %ISO 527-3
Film Elongation at Yield, TD 5.0 %ISO 527-3
Tensile Modulus 3000 MPaDry; ISO 527-1/-2
 3000 MPaConditioned; ISO 527-1/-2
Charpy Impact, Notched 2.00 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eA
 8.00 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eA
 8.00 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eA
 8.00 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eA
Tear Strength 5.00 kN/mTrouser Tear Resistance, Parallel; ISO 6383-1
 5.00 kN/mTrouser Tear Resistance, Normal; ISO 6383-1
Film Tensile Strength at Break, MD 80.0 MPaISO 527-3
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 125 °C10°C/min; ISO 11357-1/-2
 
Optical PropertiesOriginal ValueComments
Gloss 160 %60°; ISO 2813
Transmission, Visible 90 %transparent; thickness not quantified
 
Compliance PropertiesOriginal ValueComments
FDA YesFood contact
 
Descriptive Properties
Carbon Dioxide Transmission Rate, cm³/(m²*d*bar)40ISO 15105-1/-2; 23°C/ 85% RH
 90ISO 15105-1/-2; 23°C/0% RH
Elmendorf Tear Resistance, Normal (N)10ISO 6383-2
Elmendorf Tear Resistance, Parallel (N)10ISO 6383-2
Food contactEU Requirements
FormGranules
Oxygen Transmission Rate, cm³/(m²*d*bar)10ISO 15105-1/-2; 23°C/ 85% RH
 30ISO 15105-1/-2; 23°C/0% RH
PackagingCosmetics / Personal care
 Paper coating
ProcessingInjection Molding
Product AttributesBarrier Properties
 Partially aromatic Polyamide
Special CharacteristicsTransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EMS-Grivory Grivory® GTR 45 PA6I/6T
EMS-Grivory Grivory® G 21 PA6I/6T
EMS-Grivory Grivory® G 25 PA6I/6T
EMS-Grivory Grilamid® TR 55 LX PA12/MACMI
EMS-Grivory Grilamid® TR XE 4139 black 9231 PA*

PGRH311 / 157020

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.